Why do Radius Systems electrofusion fittings use exposed wire technology?
Exposed wire technology means that the metallic heating element is visible, whilst being embedded within the fitting’s body. Radius Systems consider that the exposed wire technology provides a more efficient heat transfer during the electrofusion welding process, whilst increasing joint integrity.
I want to use an electrofusion coupler as a repair coupler. Is this possible and what do I need to do? Electrofusion couplers may be used as repair couplers by removing the fitting’s centre stops; these can be cut off at the base to create a clear bore. It is important that the fitting’s internal surface, including the heating element, do not become damaged or contaminated during the removal of the stops.
Why are there 2 different terminal pin dimensions for electrofusion fittings?
Different terminal pin diameters are used for 40 and 80 Volt fittings:
• 4.0 mm terminal pins are used for 40 Volt electrofusion fittings
• 5.7 mm terminal pins are used for 80 Volt electrofusion fittings in larger diameter.
The larger diameter fittings with a 5.7mm terminal pin need a higher voltage input to make the weld using the correct control box and leads.
I have stock of Radius electrofusion fittings, but the fusion and cool times differ from entries in the brochure and on the datasheet. Why is this?
Radius Systems have a programme of continuous improvement, and this may result in changes to a fitting’s design, including changes to a fitting’s fuse and cool times.
The correct fuse and cool times for each fitting are identified on the individual packaging label. Always refer to the packaging label for the fitting’s details but if in doubt, please contact Radius Systems.
When making connections onto coiled pipes, I have noticed that the pipe has greater ovality, unlike straight pipes. What should I do to carry out an electrofusion joint?
When polyethylene pipes are supplied in coil format, there will be a greater level of pipe ovality from the coiling process, than pipe supplied in straight lengths. The coiled pipe should be re-rounded using approved re-rounding clamps in the area where the joint is going to be made.
Why do I need to prepare the pipe surface before making an electrofusion joint?
To ensure a successful welded connection is achieved, it is important that when a joint is made, no contaminants are present on the joint interface or within the welded connection. During storage, transportation, handling and installation, the external surface of a polyethylene pipe will become contaminated with dirt and debris, which must be removed before making an electrofusion joint. This is completed by using recommended pipe surface preparation techniques.
When preparing the surface of a solid wall polyethylene pipe for electrofusion jointing, what equipment
should I use?
For tapping tee connections, an industry approved ‘hand scraper’ should be used. For socket fittings, industry approved rotary pipe surface preparation tool shall be used. Such tools have the added benefit of removing a continuous layer of polyethylene material around the pipe’s circumference for the full length of the socket.
Please consult with utility tooling suppliers for recommended tooling, appropriate for the pipe diameter being prepared.
Why is it recommended to use a welding shelter when making electrofusion joints?
Welding shelters are recommended to ensure that environmental contamination on the surfaces to be joined is minimised:
• Airborne dust in dry weather
• Rain and moisture in wet conditions
When making an electrofusion joint, dust, dirt, rain and moisture act as contaminants and will reduce the quality of the electrofusion joint, if present between the pipe and fitting’s jointing surfaces.
Why do I need to use electrofusion alignment clamps?
Electrofusion alignment clamps are used for pipe to socket fitting connection and ensure that the pipe and fitting are in true alignment with one another and that there is a uniform gap between the pipe's outer surface and the fitting’s internal surface. This ensures that during the heating phase of the electrofusion process the molten material is evenly distributed around the annular gap between the pipe and the fitting to ensure joint quality.
Why do I need to use a top loading clamp when making a tapping tee connection onto a pipeline?
A calibrated top loading clamp is used with top loading tapping tees to ensure that the correct force is applied between the tapping tee body and the connecting pipe, to achieve the correct weld interface pressure during the electrofusion process.
Failure to adequately clamp the tapping tee body will result in incorrect fusion pressure and potential premature failure of the electrofusion joint.
Can I make a Tapping Tee connection onto a live polyethylene pipe?
Yes. The Radius Systems Tapping Tees are designed for live connections. After the fusion and cooling time has been completed. The outlet connection should be completed to the intended supply. The Tapping Tee joint and the outlet connection should be pressure tested prior to the commissioning process.
What equipment do I need to tap into the main?
Radius Systems' tapping tees are fitted with an integral cutter. A 12mm T Key is recommended to commission the tapping tee as it allows the application of a symmetrical torque to the tapping tee when cutting through the main. Radius Systems do not recommend the use of single arm, ratchet or power tools when commissioning tapping tees due to the potential damage.
In which position should the tapping tee cutter be, once I have commissioned the service?
The tapping tee cutter must always remain in the tapping tee. The top of the cutter should be flush with the top of the tapping tee stack.
Why is there a thread follower included with the large diameter tapping tees?
The thread follower included in all large diameter tapping tees 200 mm and above, is designed to ensure that the threads within the body of the tapping tee are not overstressed when tapping the main. It can remove be removed after the cut through has been completed. The main cutter remains in the stack and should be flush with the top after the commissioning process.
What is the recommended maximum operating pressure for Radius Systems tapping tees for gas application?
All Radius Systems gas Tapping Tee products including standard Tapping Tee’s, Purge Tee’s and Anaconda have a maximum operating pressure of 2 bar(g).
Is it normal for the Electrofusion fitting’s external surface to become hot during and immediately after the electrofusion heating cycle?
Yes, electrofusion joints are made by applying a constant voltage to the fitting’s terminal connections, which causes the fitting’s heating element to become hot. This in turn, heats the adjoining pipe surface, resulting in a homogeneous melt between the pipe and fitting. This heating process causes the fitting to become hot during and for some time after the heating cycle.Â
Why do Radius Systems' large diameter electrofusion fitting’s 450mm and above, use a 3-stage jointing process?
Radius Systems' large diameter electrofusion couplers use a 3-stage jointing process; heat - soak - weld, to
ensure that the heat between the fitting and the pipe is uniformly transferred for optimum joint quality. The 3-stage process features a pre-heat time; a heat soak time and a final weld time. The soak time is a non-energised period; it is a warming process for the fitting and pipe following the pre-heat.
Specific electrofusion control boxes capable of delivering this 3-stage process are recommended, as they feature a menu option for the 3-stage timing to be programmed and executed as a continuous process.
Why are Radius Systems' electrofusion fittings supplied with both manual (fixed) fusion time and barcode (variable) fusion time and what is the difference between them?
The manual (fixed) fusion time, which is embossed on the fitting, is intended primarily for the UK market and is suitable for electrofusion jointing at an ambient temperature range between -5°C and +23°C.
The barcode fusion time, which is variable, with built-in ambient temperature compensation, is suitable for UK and international climates within jointing temperature ranges -30°C and +50°C.
The electrofusion fitting fusion time is automatically provided based on the ambient temperature detected by the barcode enabled electrofusion control unit, where the barcode scanner is used to read the electrofusion barcode directly from the fitting label.
What if the electrofusion welding cycle cuts out before the full fusion time has elapsed?
Electrofusion control units should include software that allows the joint data to be printed out or downloaded. The data will provide an indication of the fault which has caused the electrofusion process to stop prematurely. The joint data is key to understanding the fault and should be provided to support any investigation into why the joint has been unsuccessful.Â
Electrofusion fittings that have not completed the full fusion time should be considered suspect and be removed from the pipeline for investigation until cause is established.
Is making electrofusion joints easy to complete?
Electrofusion jointing Polyethylene pipelines is a complex process. There are many differing pipe and fitting types to consider and their correct preparation. Also, there is the equipment and tooling required to correctly prepare joints. Personnel should be fully trained by a reputable utility training organisation and must have demonstrated their competency in preparing and making electrofusion joints. Personnel should also be trained in the safe systems of work associated with construction sites.
Ready to Place an Order?
Our dedicated team are ready to assist you, contact us today to discuss your project’s requirements and arrange supply. With expert guidance from first enquiry to fulfilment, we’ll help you specify the right solution and provide clear, professional support every step of the way.